Ceramic crucible
Ceramic crucibles are essential vessels for holding samples and molten materials under high-temperature conditions. The Tangshan Northern Chemical‑Physical Ceramics Industrial Zone is a major domestic production hub. Based on the alumina content of the raw material, they can be classified into two primary categories: ordinary ceramic crucibles and corundum crucibles, which differ significantly in performance and application scenarios.
Category:
Ceramics
Keyword:
Ceramic crucible
Phone:
Email:
Product introduction
Ceramic crucibles are essential vessels for holding samples and molten materials under high-temperature conditions. The Tangshan Northern Chemical and Physical Ceramics Industrial Zone is a major domestic production hub. Based on the alumina content of the raw material, they can be classified into two main categories: ordinary ceramic crucibles and corundum crucibles, which differ significantly in performance and application scenarios.
| Crucible | ||||
| Number | middle crucible | Diameter | High | Bottom base |
| C-17 | 5ml | 25 | 22 | 16 |
| C-18 | 10ml | 30 | 29 | 19 |
| C-18-1 | 15ml | 35 | 30 | 22 |
| C-20 | 20ml | 38 | 34 | 22 |
| C-21 | 25ml | 40 | 36 | 23 |
| C-22 | 30ml | 42 | 43 | 24 |
| C-23 | 40ml | 47 | 43 | 26 |
| C-24 | 50ml | 53 | 46 | 30 |
| C-24-1 | 70ml | 58 | 52 | 33 |
| C-25 | 100ml | 62 | 59 | 35 |
| C-26 | 150ml | 78 | 67 | 40 |
| C-27 | 200ml | 82 | 70 | 43 |
| C-28 | 300ml | 95 | 82 | 49 |
| Number | Low crucible | Diameter | High | Bottom base |
| C-10 | 15 low crucible | 43 | 24 | 20 |
| C-11 | 25 low crucible | 47 | 27 | 25 |
| C-12 | 30 low crucible | 50 | 30 | 25 |
| C-13 | 40 low crucible | 55 | 34 | 27 |
| C-14 | 50 low crucible | 64 | 41 | 29 |
| Number | High crucible | Diameter | High | Bottom base |
| c-1 | 15 high crucible | 32 | 35 | 20 |
| C-3 | 20 high crucibles | 32 | 44 | 20 |
| c-4 | 25 high crucible | 37 | 40 | 24 |
| C-5 | 30 high crucible | 40 | 46 | 25 |
| C-6-1 | 40 high crucible | 43 | 57 | 28 |
| C-7 | 50 high crucible | 44 | 59 | 28 |
| C-34 | 25-hole crucible | 36 | 40 | 24 |
| C-35 | 30-hole crucible | 40 | 45 | 26 |
| c-36 | 40 fine-pore crucible | 42 | 54 | 29 |
| C-37 | 50-mesh crucible | 48 | 58 | 30 |
| C-201 | New volatility | 33 | 42 | 19 |
| C-75 | 20 volatilization | 32 | 43 | 21 |
| C-76 | 25 volatilization | 37 | 46.5 | 23.5 |
| C-77 | 30 volatilization | 40 | 50 | 24 |
| C-402 | Luo Jia Guo | 40 | 40 | 22 |
| C-400 | Double-layer crucible | 32 | 41 | 20 |
| Three-pronged cauldron | 23 | 31 | 17 | |
| Carbon residue crucible | 30 | 41 | 20 | |
| Carbon-sulfur crucible | 24 | 24 | ||
| Carbon-sulfur crucible | 25 | 25 | ||
| Carbon-sulfur crucible | 26 | 26 | ||
| Number | Diameter | High | Bottom base | |
| 500 handleless dish | 132 | 67 | 82 | |
| 700 handleless dish | 142 | 86 | 83 | |
| 1000 handleless dish | 158 | 90 | 94 | |